Laboratory production of zirconium carbide compacts for ...
2008-2-29u2002·u2002Three runs with applied pressures of 1.4, 3.5, and 5.2 MPa were performed for this particular powder size. Each run had a maximum temperate hold time of 15 min. The external heat rate was adjusted to 400 °C/min to match the experiment in the first phase. The same optical pyrometers were employed to measure the temperature of the graphite susceptor and the data was subsequently …